WHITENOR® 515
White Rhodium-Ruthenium alloy solution for bath plating (ready to use)
NEWEXCLUSIVE &
PATENTED
TECHNOLOGY
RHODIUM + RUTHENIUM
L* 89.0 | a* 0.4 | b* 1.2
The pure, contemporary white.
The latest innovation in the range is WHITENOR® 515, BERKEM’s exclusive, patented plating process based on a rhodium-ruthenium alloy formulation.
This advanced technology has been developed to produce an intense, cool white finish with exceptional chromatic purity, characterised by high lightness and an extremely low yellow component.


WHITENOR® 102
White Platinum-Ruthenium alloy solution for bath plating (ready to use)
PLATINUM + RUTHENIUM
L* 88.0 | a* 0.55 | b* 2.8
The sophisticated white.
WHITENOR 102 technology combines platinum and ruthenium to produce a refined white finish, distinguished by balanced lightness and a subtle warm undertone.
A distinctive interpretation of white, designed to enhance decorative surfaces where elegance and chromatic harmony are defining qualities.
Ruthenium: The Element Driving Innovation
At the technological core of the WHITENOR range is the use of ruthenium as an alloying element, combined with either rhodium or platinum.
These two distinct metallurgical combinations move beyond the conventional monometallic approach, expanding the possibilities for engineering and defining white plated finishes.
The result is a complementary range of plating processes, each with its own distinctive chromatic identity and specific operating characteristics.
Electroplating Performance and Energy Consumption
BERKEM’s research combines the development of advanced colour characteristics with a quantitative assessment of deposition performance and the electrical energy consumption associated with electroplating processes.
102
104
515
102
| Process | Deposition rate (µm/min) |
Time for 0.2 µm | CO₂ for 0.2 µm (mg) | Time for 1 µm | CO₂ for 1 µm (mg) |
|---|---|---|---|---|---|
| RODINOR 102 | 0.15 | 80 s | 30.86 | 400 s | 154.30 |
| PLATINOR 104 | 0.12 | 100 s | 25.72 | 500 s | 128.58 |
| WHITENOR 515 — NEW | 0.15 | 80 s | 30.86 | 400 s | 154.30 |
| WHITENOR 102 | 0.05 | 240 s | 82.29 | 1,200 s | 411.47 |
CO₂ values have been calculated using an emission factor of 154.3 g CO₂/kWh, based on ISPRA reference data for the Veneto Region (2023), Table 3.3. The comparison is normalised to a surface area of 1 dm² and deposit thicknesses of 0.2 µm and 1 µm, assuming constant deposition rates.
The comparison with the conventional RODINOR 102 and PLATINOR 104 plating processes was conducted using a reference surface area of 1 dm² and two target deposit thicknesses: 0.2 µm and 1 µm.
The analysis demonstrates that WHITENOR 515 achieves a deposition rate of 0.15 µm/min, equivalent to that of the reference pure rhodium process, with the same theoretical electrical energy consumption during the deposition stage under the conditions considered.
The comparison of indirect CO₂ emissions, calculated from the electrical energy consumed, also makes it possible to quantify the differences between the processes for equivalent surface areas and coating thicknesses.
These findings highlight the importance of an integrated approach to evaluating plating technologies, taking into account chromatic quality, deposition rates and energy-related parameters.
A New Vision of White. By BERKEM.
WHITENOR Line redefines the standards of white plated finishes.
WHITENOR® LINE
Discover WHITENOR technology.
Contact BERKEM for technical and commercial information.